Materials

2660

Our 2660 crosslinked polyethylene foam has a density of 5.5 PCF / 88 kg/m³and can be used in a wide variety of applications from roofing, sports equipment to medical cushioning.

Product Description

Our 2660 crosslinked polyethylene foam has a density of 5.5 PCF / 88 kg/m³and can be used in a wide variety of applications from roofing, sports equipment to medical cushioning.

Measurements

Shore Hardness

82

Density

5.5PCF (lb/ft³)

88Kg/m³

Compression

48psi

330kPA

Service Temperature

Technical Data

Item Specs Test Method
Grade
Density (PCF) (kg/m3) 5.5 PCF
88 kg/m3
ASTM D3575
Compression Deflection (CFD)(psi)(kPa)
@25%
@50%
48 psi / 330 kPa
62 psi / 427 kPa
ASTM D3575
Shore Hardness OO (Durometer) 82 ASTM D 2240
Compression Set (%) @50% 6 ASTM D3575
Tensile Strength (psi)(kPa) 130 psi
896 kPa
ASTM D 412
Elongation (%) 200 ASTM D 412
Tear Strength Resistance (ppi) 26 ASTM D 624
Water Absorption by Weight (lb/ft2)
Accelerated Age Testing
Service Temperature (°C)(°F)
– Low
– High Continuous
– High intermittent
Flame Resistance
Industry and OEM Specifications:
Jacobs and Thompson Inc. certifies that the following
product meets the required specifications;