Materials

1294

Our 1294 neoprene blend is a 2C5 grade, black closed-cell foam used in various applications. The density is 19.0 PCF / 304 kg/m³ with a service temperature range of – 40 °F to 150 °F (high continuous use) or 200 °F (high intermittent use). This material meets the FMVSS302 FR requirement. It has a Fluid Immersion percentage of under 150%, and has good Ozone Resistance.

Product Description

Our 1294 neoprene blend is a 2C5 grade, black closed-cell foam used in various applications. The density is 19.0 PCF / 304 kg/m³ with a service temperature range of – 40 °F to 150 °F (high continuous use) or 200 °F (high intermittent use). This material meets the FMVSS302 FR requirement. It has a Fluid Immersion percentage of under 150%, and has good Ozone Resistance.

Measurements

Shore Hardness

65 - 75

Density

15 - 23PCF (lb/ft³)

240 - 368Kg/m³

Compression

17 - 25psi

117 - 172kPA

Service Temperature

-40 - 200°F

-40 - 93°C

Technical Data

ItemSpecsTest Method
Grade2C5
B3 C3 F1
2C5
II-A/B Firm
ASTM D1056-07
Suffix
SAE J 18 APR 2002
ASTM D 6576
Density (PCF) (kg/m3)15 – 23 PCF
240 – 368 kg/m3
ASTM D 1056
Compression Deflection (CFD) @25% (psi) (kPa)17 – 25 psi
117 – 172 kPa
ASTM D1056
Shore Hardness OO (Durometer)65 – 75ASTM D1056
Compression Set (%)≤ 25ASTM D 1056
Tensile Strength (psi)(kPa)150 psi
1034 kPa
ASTM D412
Elongation (%)175ASTM D412
Tear Strength Resistance (ppi)35ASTM D 624
Water Absorption by Weight %<5ASTM D1056
Accelerated Age Testing:
7 Days @ 158 °F Chang in CD
± 30% maxASTM D1056
Service Temperature (°C)(°F)
– Low
– High Continuous
– High intermittent
-40°C | -40°F
65°C | 150°F
93°C | 200°F
Flame ResistancePassFMVSS302
Industry and OEM Specifications:
Jacobs and Thompson Inc. certifies that the following
product meets the required specifications;
ASTM D 1056-14 2A5 2C5
WSK M2D 419-A Type 6
GMW15473 Class I Type VI