1120
Our 15 pcf / 240 kg/m³ 1120 epichlorohydrin (ECH) closed-cell foam provides excellent chemical, ozone and oil resistance, plus one of the most versatile temperature ranges (-20 F to 325 F or -29 C to 163 C). At low temperatures, ECH shows excellent aging, resiliency, and flexibility characteristics. It has a Fluid Immersion rate under 50%.
Product Description
Our 15 pcf / 240 kg/m³ 1120 epichlorohydrin (ECH) closed-cell foam provides excellent chemical, ozone and oil resistance, plus one of the most versatile temperature ranges (-20 F to 325 F or -29 C to 163 C). At low temperatures, ECH shows excellent aging, resiliency, and flexibility characteristics. It has a Fluid Immersion rate under 50%.
Measurements
| Shore Hardness | 35 - 45 |
|---|---|
| Density | 12 - 18PCF (lb/ft³) 192 - 288Kg/m³ |
| Compression | 2 - 5psi 13.7 - 34.4kPA |
| Service Temperature | -40 - 325°F -40 - 162°C |
Technical Data
| Item | Specs | Test Method |
| Grade | 2B1 2B1 | ASTM D1056 SAE J-18 APR2002 |
| Density (PCF) (kg/m3) | 12 – 18 PCF 192 – 288 kg/m3 | ASTM D 3676 |
| Compression Deflection @25% (CFD) (psi) (kPa) | 2 – 5 psi 13.7 kpa – 34.4 kPA | ASTM D 1056 |
| Shore Hardness OO (Durometer) | 35 – 45 | ASTM D 2240 |
| Compression Set @25% | ≤ 25 | ASTM D 1056 |
| Tensile Strength (psi) (kPa) | 120 psi 827 kPa | ASTM D 412 (Die A) |
| Elongation % | 250 | ASTM D 412 (Die A) |
| Tear Strength Resistance (ppi) | 18 | ASTM D 412 (Die C) |
| Water Absorption by Weight % | <5 | ASTM D 1056 |
| Accelerated Age Testing Oven Aged 7 Days @ 158 °F Change in CFD (%) | ± 30% | ASTM D 1056 |
| Service Temperature (°C)(°F) – Low – High Continuous – High Intermittent | -40°C | -40°F -148°C | -300°F -162°C | -325°F | ASTM D 746 |
| Flame Resistance | Pass | FMVSS 302 |
| Industry and OEM Specifications: Jacobs and Thompson Inc. certifies that the following product meets the required specifications; | MS-AY432 GMW15473 CLASS 1 TYPE 5 ASTM D 1056-07 2B1 GM 6086M Type IIIA; ASTM D 1056-00 2B1 |